My Posts This: Topic Forum | Sometimes de-stressing the plastic by boiling it in water for a minute or so helps... Sounds odd I know, but it helped with mine!
Directly after the injection moulding process the plastic can slightly distort in shape, re-heating it in boiling water and allowing it to cool will often allow it to assume its intended shape if indeed it was distorted in the first place. |